Title: |
US5954969:
Recovery of iron oxides from polluted coal mine drainage
[ Derwent Title ]

|
Country: |
US United States of America

|
| |
Inventor: |
Hedin, Robert S.; Pittsburgh, PA 15228

|
Assignee: |
None

|
Published / Filed: |
1999-09-21
/ 1997-04-15

|
Application Number: |
US1997000834236

|
IPC Code: |
Advanced:
C02F 1/64;
Core:
C02F 1/62;
IPC-7:
C02F 1/64;

|
ECLA Code: |
C02F1/64C;

|
U.S. Class: |
Current:
210/709;
210/170.07;
210/201;
210/205;
210/253;
210/322;
210/722;
210/724;
210/747;
423/140;
423/633;
Original:
210/709;
210/722;
210/724;
210/747;
210/170;
210/201;
210/205;
210/253;
210/322;
423/140;
423/633;

|
Field of Search: |
210/96.1,101,198.1,199,170,200,709,722,724,747,201,205,253,322
423/140,633

|
Priority Number: |
| 1997-04-15 |
US1997000834236 |
| 1996-04-15 |
US1996000015976P |

|
Abstract: |
A method and system is provided for producing a commercially usable iron oxide material by treating iron contaminated water. A clean effluent is also produced. Iron contaminated water is sampled to determine a bicarbonate to iron molar ratio. The flow of the water is directed to a collection basin assembly when the bicarbonate to iron molar ratio is at least 2 to 1. Iron oxide material precipitates in the collection basin assembly. The water from the collection basin assembly is directed to a constructed wetland. After a period of time, the iron oxide material in the collection basin assembly can be harvested and used for commercial purposes without excessive further treatment.

|
Attorney, Agent or Firm: |
Webb Ziesenheim Logsdon Orkin & Hanson, P.C. ;

|
Primary / Asst. Examiners: |
Woo, Jay H.; Prince, Fred

|
Maintenance Status: |
CC Certificate of Correction issued

|
INPADOC Legal Status: |
Show legal status actions

|
Parent Case: |
CROSS REFERENCE OF RELATED APPLICATION
This application claims the benefit of Provisional Application No. 60/015,976 filed on Apr. 15, 1996.

|
Family: |
None

|
First Claim:
Show all 20 claims |
I claim:
1. A method for producing and recovering an iron oxide material from alkaline, iron containing water, comprising the steps of:
- sampling the iron containing water to determine a bicarbonate to iron molar ratio;
- transporting the sampled water to a collection basin assembly having at least one collection basin when the bicarbonate to iron molar ratio is at least about 2 to 1;
- preventing contamination of the sampled water in the collection basin assembly;
- precipitating an iron oxide material in the at least one collection basin; and
- recovering the precipitated iron oxide material by removing the precipitated iron oxide material from the at least one collection basin.

|
Background / Summary: |
Show background / summary

|
Drawing Descriptions: |
Show drawing descriptions

|
Description: |
Show description

|
Forward References: |
Show 6 U.S. patent(s) that reference this one

|